极地船波纹换热管冲蚀磨损研究与防护
徐立,孙强,刘宏刚,汤冰,黄长绪
0
高性能船舶技术教育部重点实验室武汉理工大学,湖北 武汉 430063;武汉理工大学能源与动力工程学院,湖北 武汉 430063
摘要:针对极地船波纹管换热器中进入冰晶颗粒对管路产生严重腐蚀磨损问题,采用CFD中欧拉-拉格朗日离散框架的DPM模型及腐蚀磨损模型研究流速、冰晶颗粒直径和含冰率条件变化对水平直波纹管磨损特性的影响。结果表明:波纹管磨损严重位置发生在波纹与直管衔接处、波谷处以及与流速相对的波峰面,且出口直管段磨损最为严重,而水平光滑圆管顶部位置磨损比较严重,但波纹管的磨损率均大于相同条件下光滑直管的磨损率;流速对磨损率影响最大,可使波纹管使用寿命减少10倍以上;冰晶颗粒直径对波纹管磨损影响较小;含冰率对管壁磨损也有很大影响,含冰率为10%时波纹管使用寿命比含冰率为2%时的减少4.2倍。根据以上研究结果提出了相应的防护措施。
关键词:  极地船  波纹管换热器  腐蚀  磨损率
Research and Protection of Erosion of Corrugated Heat Transfer Tubeson Polar Ships
Xu Li,Sun Qiang,Liu Honggang,Tang Bing,Huang Changxu
Key Laboratory of High Performance Ship Technology Wuhan University of Technology,Ministry of Education,Hubei Wuhan 430063;School of Energy and Power Engineering,Wuhan University of Technology,Hubei Wuhan 430063
Abstract:In order to solve the problem of severe erosion of the corrugated heat exchanger on the polar ship, using the DPM model of Euler-Lagrangian discrete frame in CFD and the erosion wear model to analyze the effects of different inlet velocities, ice particle diameters and ice contents on the wear characteristics of horizontal straight corrugated tubes. The numerical results show that:the location of severe wear occurs at the interface between the corrugated and the straight tube section, the trough, and the crest surface against the flow,and the export section of the straight tube wore down the most severely, and the top of horizontal somooth circular tube is relatively serious; the erosion rate of corrugated tube is larger than the erosion rate of smooth straight tube under the same condition; the flow velocity has largest impact on erosion rate and can reduce the service life of corrugated tube by more than 10 times; the effect of ice crystal diameter on the wear of corrugated tube is small, the ice content also has a great influence on wall erosion, when ice content is 10% ,service life of corrugated tube decreases by 4.2 times than ice content of 2%.The protective measures are given according to the research.
Key words:  polar ship  corrugated heat transfer tube  erosion  wear rate